Metal materials · selection guide · for R&D and purchasing
Both are called “iron-nickel alloy,” yet the 36% nickel grade barely expands with heat, while the 80%-nickel class has magnetic permeability tens of times that of ordinary steel. A small change in composition, a completely different use.
Nickel alloy inquiries often say only: “I need iron-nickel alloy sheet.” But iron-nickel is not one material — the same two elements in different ratios solve entirely different engineering problems: one keeps thermal expansion close to zero, another carries magnetic fields away. This article lines up JIAHON’s six stock nickel alloys by the problem each solves, and explains how pure nickel mainly differs from copper, aluminium and titanium.
1. Six nickel alloys, each solving one problem
| Alloy (composition, wt%) | Problem it solves | Key figure | Common uses | Stock thickness |
|---|---|---|---|---|
| Iron-nickel Fe64Ni36 (low-expansion alloy) | Thermal expansion | Coefficient of thermal expansion about 1.2 ppm/°C (20–100 °C) | Precision gauges, optical mounts, instrument structures, composite molding tools | 0.02–3 mm |
| Iron-cobalt-nickel Fe54Co17Ni29 (glass-sealing alloy) | Expanding together with glass | About 5 ppm/K (30–200 °C), matched to borosilicate glass | Hermetic glass-to-metal seals, vacuum devices, electronic packaging | 0.02–2 mm |
| Iron-nickel Fe15Ni85 (high-nickel permalloy class) | Guiding and blocking magnetic fields | Typical permalloy (about 80% nickel) has relative permeability around 100,000 (ordinary steel a few thousand); actual values depend on composition and heat treatment | Magnetic shielding, magnetic cores, sensors | 0.05–3 mm |
| Iron-nickel Fe50Ni50 (medium-nickel soft magnetic) | Soft magnetic parts | Belongs to the 45–50% nickel permalloy family | Soft magnetic components, magnetic circuit parts | 0.1–3 mm |
| Nickel-chromium Ni80Cr20 | Heating with current | Resistivity about 1.12 μΩ·m (about 66 times copper), melting point about 1,400 °C | Electric heating elements, heater sheets | 0.03–2 mm |
| Nickel-copper-zinc Ni18Zn24Cu58 (nickel silver) | Corrosion resistance with a silvery look | Copper-based alloy; “silver” in the name but contains no silver | Springs, contacts, decorative parts | 0.02–3 mm |
Values are standard reference figures for each alloy class; go by the mill certificate for each batch. This series is supplied as precision thin sheets by composition ratio.
2. Why a small difference in composition means they can’t be swapped
Fe64Ni36 and Fe15Ni85 both contain only iron and nickel, but the first is valued because its dimensions don’t change with temperature, and the second because magnetic flux passes through it easily. Use the Fe64Ni36 low-expansion alloy for magnetic shielding, or high-nickel permalloy for precision gauge structures, and both will fail.
The Fe54Co17Ni29 glass-sealing alloy takes another approach: it is not meant to “not expand,” but to “expand together with glass.” Its coefficient matches borosilicate glass, so once glass and metal are sealed, both expand and contract together through temperature cycles and the seal doesn’t crack.
In one line: stay still → Fe64Ni36 low-expansion alloy; move with glass → Fe54Co17Ni29 glass-sealing alloy; block magnetic fields → high-nickel permalloy class (Fe15Ni85); heat up → nickel-chromium (Ni80Cr20).
So when inquiring, give the composition ratio rather than just “iron-nickel alloy.” With the composition clear, plus thickness and size, quotes and deliveries won’t go wrong.
Related products: metal alloy sheet series (iron-nickel / nickel-copper-zinc / iron-cobalt-nickel / nickel-chromium sheet).
3. Pure nickel: the main difference from copper, aluminium and titanium is magnetism
Like iron and cobalt, nickel is ferromagnetic at room temperature, with a Curie temperature of about 355 °C. So pure nickel is attracted by magnets — completely unlike copper, aluminium and titanium. Where magnetic fields matter, nickel is not a non-magnetic option.
Nickel forms a passive oxide film that protects it; in caustic alkali solutions (such as sodium hydroxide), nickel and nickel alloys are among the most corrosion-resistant metals. That is why nickel mesh and nickel foam appear so often in alkaline electrochemistry and battery research — the positive electrodes of rechargeable nickel-cadmium and nickel-metal hydride batteries use nickel hydroxide.
Pure nickel has a density of 8.907 g/cm³ and melts at 1,455 °C.
Related products: metal sheet series (nickel sheet), metal mesh series (nickel mesh), metal tube series (nickel tube), metal foam series (nickel foam).
4. Match your need in the table
| Your need | Material | Product on our site |
|---|---|---|
| Dimensions must not change with temperature (gauges, optics, molds) | Fe64Ni36 low-expansion alloy | Metal alloy sheet series |
| Hermetic glass-to-metal seals, vacuum devices | Fe54Co17Ni29 glass-sealing alloy | Metal alloy sheet series |
| Magnetic shielding, cores, sensors | High-nickel permalloy class (Fe15Ni85) | Metal alloy sheet series |
| Electric heating elements, heater sheets | Nickel-chromium (Ni80Cr20) | Metal alloy sheet series |
| Springs, contacts, silvery appearance | Nickel silver (Ni18Zn24Cu58) | Metal alloy sheet series |
| Alkaline electrochemistry, battery electrodes, current collectors | Pure nickel (mesh / foam / sheet) | Nickel mesh, nickel foam, nickel sheet |
| Winding, electrode leads | Pure nickel wire | Metal wire series (nickel wire) |
| Evaporation and melting feedstock | Pure nickel pellets | Metal pellet series (nickel pellets) |
| Welding nickel alloys | Nickel alloy welding electrodes | Nickel alloy welding electrodes |
5. FAQ
What is the difference between the Fe64Ni36 low-expansion alloy and the Fe54Co17Ni29 glass-sealing alloy? The Fe64Ni36 low-expansion alloy is about “staying still”: its expansion coefficient is about 1.2 ppm/°C (20–100 °C), for precision gauges, optical mounts and molding tools whose dimensions must be stable. The Fe54Co17Ni29 glass-sealing alloy is about “moving with glass”: about 5 ppm/K, matched to borosilicate glass, for hermetic glass-to-metal seals. They can’t be swapped.
Is nickel attracted to magnets? Yes. Nickel is ferromagnetic at room temperature (Curie temperature about 355 °C) and is attracted by magnets like iron and cobalt. Where non-magnetic materials are needed, use pure copper, aluminium or titanium. Further reading: Pure titanium or titanium alloy TC4? (titanium is non-ferromagnetic).
Why is nickel-chromium good for heating elements? Two reasons: high resistivity, about 1.12 μΩ·m or about 66 times copper, so it heats readily with current; and when heated red-hot it forms a chromium oxide layer that is very stable in air and almost impermeable to oxygen, protecting the base metal from further oxidation.
Does nickel silver (nickel-copper-zinc) contain silver? No. Nickel silver, also called German silver, is named for its silvery-white look; its actual composition is copper, nickel and zinc (Ni18Zn24Cu58 in this series). It is a copper-based alloy and a close relative of cupronickel (copper-nickel) discussed in our copper materials article. Further reading: Copper, brass, bronze or cupronickel: how to choose.
What information should I give when inquiring? The composition ratio (for example Fe64Ni36, not just “iron-nickel alloy”), thickness, size and quantity, plus one line on the use — low expansion, sealing, magnetic permeability or heating. With the use stated, we can help confirm the composition choice. Small quantities for research and trials are welcome.
Please contact JIAHON or email [email protected].