中文English

How Tightly to Control Plant Temperature and Humidity: Which Conditions Matter for Solder Paste, Moisture-Sensitive Parts, and ESD — 5 Stages from Setting a Window to Audits

No public standard gives SMT plants one general set of temperature and humidity numbers; what needs doing is to list the separate conditions for solder paste, moisture-sensitive parts, and ESD, take the overlapping range as the window, and then manage it in two levels: “alarm” and “shutdown.”

  • Each of the three conditions has its own documents: for solder paste, look at the use environment in the datasheet; the exposure time (floor life) of moisture-sensitive parts assumes the plant is at or below 30°C / 60% RH (relative humidity); the EOS/ESD Association (ESDA) says ANSI/ESD S20.20 does not require humidity control, but if your control program specifies humidity, it must be monitored.

  • There are reference ranges for the numbers: according to Jiahon’s earlier reference data, a common on-site alarm window is about 18–27°C and 40–65% relative humidity; the shutdown line is set a little wider outside the alarm line. This is on-site experience, not a standard.

  • Fluctuation matters more than the average: according to Jiahon’s earlier reference data, humidity that stayed within specification but swung back and forth once dragged down yield; what audits often ask is whether there is a range, whether there are records, and what is done when limits are exceeded.

For airborne dust (foreign matter in the air), see “Does SMT Dust Need Controlling? 5 Types of Foreign Matter to Control and Line Discipline“; for timing and baking after parts are unpacked, see “Storage and Baking Conditions for Moisture-Sensitive Devices“. This article starts from “where should the temperature and humidity of this plant actually be set,” and covers only temperature and humidity. Each stage below describes how to do it and how Jiahon can help; sources and exceptions are in the notes at the end.

Use environment in the solder paste datasheet

Assumption for moisture-sensitive parts (upper limit only)

If the ESD program specifies a range

Relative humidity low → high
Temperature low → high

Plant window
Where the three overlap

Then split into
two levels
What to do when it is exceeded: manage in two levels

Alarm: someone must act
Within window
Normal
Shutdown: no production
Orange line = alarm line Red dashed line = shutdown line

① List the three conditions

② Take the overlap to set the window

③ Split into alarm and shutdown

④ Where to measure, how to record

⑤ Watch fluctuation, prepare for audits
Schematic: the size and position of the boxes do not represent actual values

Figure 1 Take the overlap of the three conditions to set a window, then split into alarm and shutdown levels

Stage ①: List What Each of the Three Conditions Requires

Temperature and humidity are not one number but the separate requirements of three things. Look at them separately first, then put them together.

What to controlIts temperature and humidity requirementWhere to find it
Solder pasteHow long it can be used on the stencil, and whether prints slump, are both affected by temperature and humidity. One public datasheet for a lead-free no-clean solder paste states that a stencil life of over 8 hours assumes 22–28°C and 30–60% RHThe use conditions section of the solder paste datasheet
Moisture-sensitive parts and circuit boardsExposure time assumes the plant is at or below 30°C / 60% RH; if more humid or hotter, the time must be reducedJ-STD-033; “Storage and Baking Conditions for Moisture-Sensitive Devices”
ESDHumidity is not a requirement of ANSI/ESD S20.20; but if the program specifies a humidity range, it must be monitored, recorded, and given an out-of-limit procedureESD control program, customer specifications

Solder paste: the use environment stated in the datasheet should be treated as a requirement of that paste, not a reference. Papers use temperature and humidity directly as test conditions: some measure slump at different humidities, once right after printing and again after 2 hours; some place printed boards at 30°C / 80% RH for two hours to see whether bridging increases, as a hot and humid case. Water-soluble pastes are more sensitive to temperature and humidity: one paper mentions that water-soluble types generally have a shorter stencil life; in a comparison of 6 pastes, the water-soluble types had a narrower printing window, and when left in ambient conditions between printing and reflow, solder balling got worse, while no-clean types were unaffected.

Moisture-sensitive parts: the 30°C / 60% RH for exposure time is an assumption, not a target for the plant. If the plant is more humid or hotter than that, convert the number of days using the tables in J-STD-033; for details, see the article above. There is also an often overlooked phenomenon: when a cold object meets humid air, condensation forms. At 28°C and 70% RH in the plant, the air’s dew point is about 22°C, and a solder paste jar just taken out of the refrigerator is only a few degrees, so condensation will certainly form the moment it is opened (see the dew point table in the notes). So solder paste should be warmed up sealed in its jar and opened only once it reaches room temperature; for how, see “How Long to Stir Solder Paste? How to Set the Use Period After Opening“.

ESD: ESDA’s explanation is that humidity helps reduce charge buildup but is not enough to lower the risk; at room temperature, between 20% and 30% RH, the difference in charge buildup on insulating materials is very small, so S20.20 does not rely on humidity. ESD materials and items are verified under very dry conditions (12% ± 3% RH, 23°C ± 3°C), and once they pass, there is no need to rely on humidity control. The new edition of S20.20 also allows a plant to verify instead at “the dry humidity of the year” for that plant. The mainstays of ESD control are grounding, ESD materials, and ionization; see “The Complete Guide to ESD Protection“; humidity is just one of the environmental conditions.

How Jiahon can help:

  • Solder Paste / Solder Wire Series: the page lists SAC305, Type 4 powder, and halogen-free solder pastes, as well as solder wire in various specifications; for each one’s use environment and datasheet, please inquire.

  • Temperature and Humidity Test Chamber: if you want to verify how a given solder paste or part behaves on the humid days in your plant, you can put samples in to simulate them. The 260-liter model has a temperature control range of 0–70°C, humidity of 30–98% RH, and 24 programmable segments; for other capacities and customization, please inquire. A test chamber is for testing and cannot be used to control a whole plant.

  • Ultra-Low Humidity Electronic Dry Cabinet: on days when the plant’s humidity cannot be kept in the window, moisture-sensitive parts go in here separately; there are two levels, 1%–10% RH and 1%–3% RH. For how to choose, see “Dry Cabinet vs. Nitrogen Cabinet“.

Stage ②: Take the Overlapping Range to Set Your Own Window

Once the three conditions are listed, the method is:

  • List the solder pastes first: list the use environment of each solder paste used in this plant.

  • Then add other conditions: the assumption for moisture-sensitive parts (at or below 30°C / 60% RH), and any ranges written in customer specifications.

  • Take the overlap: the overlapping part is the window.

  • Put the setpoint in the middle: do not sit against the edge. If the air conditioning is set at the edge, the slightest drift takes it out.

The figures in the table below are two hypothetical solder pastes; they only demonstrate the method, not measurements.

Condition sourceTemperatureRelative humidity
Datasheet of solder paste A22–28°C30–60%
Datasheet of solder paste B20–26°C40–60%
Assumption for moisture-sensitive parts30°C or below60% or below
Overlap (window)22–26°C40–60%
Setpoint (middle)24°C50%

According to Jiahon’s earlier reference data: the ambient temperature requirements of several solder pastes compared fell between about 18–27°C, differing from paste to paste; the earlier data put the setpoint near the middle of each paste’s window. Another on-site environmental control specification has a common alarm window of about 18–27°C and about 40–65% relative humidity, narrower in higher-cleanliness areas, about 20–24°C and 40–60%; the humidity alarm for warehousing and incoming areas is about 70%. These are on-site experience from a single specification, with no public document to compare against; your window should be set according to your own solder pastes, parts, and customer specifications.

Two reminders:

  • An upper limit of 65% is wider than the exposure-time assumption: the earlier data’s humidity upper limit is about 65%, higher than 60%. This is an inference from comparing the two numbers: if the window’s upper limit is set at 65%, the exposure time of moisture-sensitive parts needs to be converted separately; for simplicity, tighten the upper limit to 60%.

  • The window must be written down: which area, what the temperature and humidity are, and which datasheet or specification it is based on. A window that exists only in the air conditioning technician’s head cannot be produced at an audit.

How Jiahon can help: this stage is data-organizing work; there is nothing to buy.

Stage ③: Manage in Two Levels: Alarm and Shutdown

A window only answers “what is normal,” not “what to do when it is exceeded.” The earlier data’s approach is two levels:

  • Alarm: outside the window, someone must act: notify the person responsible, find the cause, and keep a record.

  • Shutdown: a further margin beyond that, and production in that area is not allowed.

AreaAlarm windowShutdown line
General assembly areaTemperature about 18–27°C; relative humidity about 40–65%Wider than the alarm line: about 2°C for temperature, about 2–5 percentage points for humidity
Higher-cleanliness areaTemperature about 20–24°C; relative humidity about 40–60%Same as above
Warehousing and incoming areaRelative humidity upper limit about 70%Same as above

This table is on-site experience compiled by Jiahon from earlier reference data, not a standard. What to remember is the structure: two levels, each with a person responsible and a response time.

What to do after a limit is exceeded should also be written in advance. When discussing low humidity, the ESD Association says the magnitude of the change and how long it lasts are key. Humidity more than 3% RH below the limit that lasts only a few minutes is low risk; if it lasts for several hours, it may count as nonconforming. In that case, gather objective evidence to judge whether ESD-sensitive items can still be handled; if the limit is judged to have been exceeded, stop handling ESD-sensitive items and keep the evidence as a record. This logic can be borrowed to set the procedure for temperature and humidity: how far over, for how long, and which path each takes.

How Jiahon can help:

  • Temperature and Humidity Transmitter: wall-mounted, with a polymer capacitive humidity sensor and an LCD showing temperature and relative humidity together; humidity measurement 0–100% RH (non-condensing), accuracy ±2% (10–90% RH) or ±3% (standard model); optional 4–20 mA or 0–10 V output to connect to the facility controller. The temperature measurement range depends on the model; please inquire.

  • The alarm and shutdown logic is done by the facility’s controller or monitoring system; Jiahon supplies the sensing end. Jiahon has no product pages for air conditioning, humidification, or dehumidification units; please contact your facilities team or an air conditioning contractor.

Stage ④: Where to Measure, How Often, and How to Record

Once the window and alarm lines are set, it only counts as control when someone measures and there are records.

  • Location: windows are set by area, with at least one measurement point per area. Install where the airflow is representative, away from heat sources, air outlets, and dead corners; the product page for the wall-mounted unit recommends about 1.2–1.5 meters above the floor.

  • Frequency: according to Jiahon’s earlier reference data, temperature and humidity are measured about once per shift (dust about weekly; see the separate article on dust). To see how it changes over a day, record continuously with a data logger, with a shorter sampling interval.

  • Records: handwritten records should have at least the time, reading, and person measuring; with a data logger, it should be possible to export and retain the data.

  • Instruments: measuring instruments should be calibrated regularly, with records kept. An instrument with inaccurate readings leaves the whole control system without a basis.

  • Spot checks: handheld measuring instruments can be used for on-site spot checks, and also to cross-check the readings of fixed sensors.

How Jiahon can help:

  • Temperature and Humidity Data Logger: two channels (temperature, humidity), temperature ±0.3°C, humidity ±2.5% RH, memory of 8,000 readings × 2 channels, sampling interval 1 second to 60 minutes; built-in WiFi, and can be used with the maker’s cloud platform for remote monitoring and alarm notifications (please inquire about the platform and fees); powered by 4 AA batteries or USB.

  • Handheld Measuring Instrument Series: the page lists air quality meters (measuring temperature, humidity, and PM2.5), particle counters, infrared thermometers, and more; for the specifications of each model, please inquire.

Stage ⑤: Watch Fluctuation, and Prepare What Audits Will Ask

Fluctuation: an average within the window does not mean there is no problem. According to Jiahon’s earlier reference data, a relocation assessment report once wrote that humidity swinging back and forth within specification dragged down yield; how long it takes humidity to return to range depends on the heaters, humidifiers, and the airtightness of the plant. When looking at data logger curves, you can check whether swings coincide with doors opening, shift changes, or air conditioning starting and stopping.

Cold things entering the plant: refrigerated solder paste and material taken from cold storage will certainly get condensation when their temperature is below the plant’s dew point. For solder paste, warm it up sealed in its jar and open it only once it reaches room temperature; for other cold material, also wait until it is close to room temperature before unpacking.

Audits: according to Jiahon’s earlier reference data, a customer audit once listed “no temperature and humidity control” as a finding. The table below is compiled from the ESD Association’s explanation of humidity control (monitoring, objective evidence, an out-of-limit procedure) and this type of finding; it is not the text of an audit checklist.

What audits askWhat to prepare
Is there a specified range?A written window for each area (Stage ②)
What happens when it is exceeded?Alarm and shutdown levels, with persons responsible and response times (Stage ③)
Is it measured, and accurately?Measurement locations, frequency, instrument calibration records (Stage ④)
Are there records?Continuous records or per-shift records, retained for a period
What was done the time it was exceeded?Records of time, cause, action, and closure
Does the window match the material documents?Cross-reference of solder paste datasheets, J-STD-033, and customer specifications

How Jiahon can help:

  • Solder Paste Warm-Up Unit: sealed warm-up for 500-gram solder paste jars, with each station’s temperature independently settable and alarmed; the page also summarizes dew point and condensation.

  • Temperature and humidity data logger: as in Stage ④; the curves and out-of-limit records are exactly the data an audit looks at.

If you need temperature and humidity data loggers, transmitters, handheld measuring instruments, dry cabinets, solder paste warm-up units, or temperature and humidity test chambers, you are welcome to contact Jiahon.

Further reading
To look at the related process steps together, you can go on to read:

Notes: Sources and Exceptions

The following is for those who need to verify; skipping it does not affect the method above. For the clauses and table numbers of standards, refer to the official text; where the edition you use, customer specifications, or solder paste maker documents differ, they take precedence.

Sources for each practice

PracticeContentSource
Solder paste and humidity testingA paper summarizing others’ methods: slump measured at different humidities right after printing and after 2 hours; solder balling measured by leaving printed boards at different humidities for 2 hours before reflowLentz (citing Anson et al.)
Hot and humid casePrinted boards placed in a static oven at 30°C / 80% RH for 2 hours, recording whether bridging increasedFarrell et al.
Water-soluble types more sensitiveA comparison of 6 solder pastes: water-soluble types are sensitive to temperature and humidity and have a narrower printing window; left in ambient conditions between printing and reflow, water-soluble solder balling got worse, while no-clean types were unaffectedGuéné and Teh
Exposure-time assumptionThe exposure time for each moisture sensitivity level (MSL) assumes the plant is at or below 30°C / 60% RH; when more humid or hotter, convert using Table 7-1. This site read only the standard’s table of contents; for the values in the table, see the official textJ-STD-033D (see the notes in “Storage and Baking Conditions for Moisture-Sensitive Devices”)
ESD and humidityHumidity is not a requirement of S20.20; materials are verified at 12% ± 3% RH, 23°C ± 3°C; if the program specifies humidity, it must be monitored, with evidence kept and an out-of-limit procedure; between 20% and 30% RH the difference in charge buildup on insulating materials is very small; the new edition allows verification at the plant’s dry humidity of the year; the magnitude and duration below the limit are the key risk factorsESDA FAQ, ESDA article
Dew pointCalculated with the Magnus approximationAlduchov and Eskridge; the U.S. weather service’s dew point calculation page

This is the general case; individual situations still need to be assessed case by case.

Dew point table

The following dew points are calculated with the Magnus approximation (constants 17.62 and 243.12°C), in °C; using other common constants, the results differ by less than 0.1°C. When an object’s surface is colder than the dew point, water vapor condenses on it.

Room temperatureRH 50%RH 60%RH 70%RH 80%
22°C11.113.916.318.4
25°C13.916.719.121.3
28°C16.619.522.024.2
30°C18.421.423.926.2

Exceptions and limits

  • The earlier data’s ranges are a single source: the alarm window, the width of the shutdown line, and the measurement frequency come from one on-site specification in Jiahon’s earlier reference data, with no public document to compare against; they are on-site experience, not a standard; the window for each area should be set according to your solder pastes, parts, and customer specifications.

  • Figures in the demonstration table: the two solder pastes in Stage ② are hypothetical and only demonstrate the method of taking the overlap.

  • Papers are not your product: the solder pastes, equipment, and dates in the papers all differ, and the results cannot be applied directly to your product.

  • ESD: ESDA’s explanation is for control programs under S20.20 and IEC 61340-5-1; customer specifications may separately state humidity requirements, in which case customer specifications take precedence.

  • Dust: ISO 14644-1 covers the classification of airborne particles, not temperature and humidity; see “Does SMT Dust Need Controlling?”.

  • A test chamber is not air conditioning: a temperature and humidity test chamber is for testing and cannot be used to control the temperature and humidity of a whole plant.

  • Equipment: Jiahon has no product pages for air conditioning, humidification, or dehumidification units.

Standards cited
For the standards cited in this article, please refer to the current edition from each issuing body.

This article is a summary of the general case. It is not a restatement of standard clauses or papers, and does not constitute an endorsement of your process. For your plant’s temperature and humidity window, rely on the edition of J-STD-033 you use, solder paste maker documents, customer specifications, and your own verification; this is the general case, and individual situations still need to be assessed case by case.

Back to top