中文

Stainless Steel 201, 304, 316, 316L: How to Choose — Composition, Corrosion Resistance and Magnetism Explained in One Page

Metal materials · Selection guide · Must-read for R&D and purchasing

“If a magnet picks it up, it is fake stainless steel” is a common misunderstanding: 430 is real stainless steel, and it is magnetic by nature.

By the Jiahon affiliated-company engineering team · about 7 minutes to read

Stainless steel is not one material but a whole family. If a drawing says just “stainless steel” with no grade, what gets made can be two things that differ by twice the cost and one grade of corrosion resistance. What really decides the grade is two questions: whether there are chloride ions in the environment, and whether the part is to be welded.

This article puts the composition and differences of the common grades on one table, and explains what magnetism actually tells you.

1. Comparison table of common grades

GradeMain composition (wt%)StructureCharacteristicsCommon uses
201Cr 16–18 | Ni 3.5–5.5 | Mn 5.5–7.5 | C ≤0.15 | N ≤0.25AusteniticManganese and nitrogen partly replace nickel, so cost is lower; corrosion resistance is weaker than 304Indoor structures, supports in non-corrosive environments
304Cr 17.5–19.5 | Ni 8.0–10.5 | C ≤0.07AusteniticGeneral purpose, with a good balance of corrosion resistance and workabilityGeneral equipment, fixtures, kitchen and indoor appliances
304LCr 17.5–19.5 | Ni 8.0–12.0 | C ≤0.030AusteniticLow carbon, reducing weld sensitization (chromium carbide precipitating at grain boundaries)Parts that are welded and still need corrosion resistance after welding
316Cr 16–18 | Ni 10–14 | Mo 2–3AusteniticContains molybdenum; resistance to chloride pitting and reducing acids is better than 304Chloride environments, chemical processing, seaside, medical
316LCr 16–18 | Ni 10–14 | Mo 2–3 | C ≤0.030AusteniticThe low-carbon version of 316, keeping corrosion resistance after weldingWelded chemical parts, laboratory ware, metal mesh
430Cr 16–18 | Ni ≤0.75FerriticNo nickel; good formability but lower corrosion and temperature resistance; magneticDecorative parts, appliance exteriors (Jiahon does not list this grade)

Composition follows the specification ranges of ASTM A240/A240M (plate, sheet and strip); the ranges for tube and other specifications, and for same-named grades in JIS and GB, are not exactly the same, and for an actual lot the material certificate prevails. Jiahon’s stainless steel items cover 201 / 304 / 316 / 316L; 430 is not listed.

2. Two questions decide which one you need

2.1 Are there chloride ions in the environment?

This is the one dividing line that really matters between 304 and 316. 316 contains 2–3% molybdenum and tolerates both the local pitting caused by chloride ions and reducing acids such as sulfuric acid better than 304. Seaside, chlorinated cleaning fluids, electrolytes, swimming pool environments, some food processing — in these places 304 shows spot rust, and that is not “a dirty surface” but pitting.

Conversely, in a dry indoor environment, for general mechanism parts and fixtures, 304 is enough, and changing to 316 just costs more.

2.2 Is this part to be welded?

If it is to be welded, choose the L (low-carbon) version. The carbon limit of 304 is 0.07%, and 304L presses it to 0.030%; in a stainless steel with higher carbon, in the temperature range of welding, chromium precipitates at the grain boundaries as chromium carbide, the chromium in that ring is used up and corrosion resistance drops; this is called sensitization. The L version keeps the carbon low to avoid this.

The combinations of the two questions: no chlorine, no welding → 304 | no chlorine, welding → 304L | chlorine, no welding → 316 | chlorine and welding → 316L

› Related products: Metal Sheet Series (Stainless Steel Sheet), Metal Rod Series (Stainless Steel Rod), Metal Wire Series (Stainless Steel Wire), Metal Mesh Series (316L Stainless Steel Mesh)

3. Frequently asked questions

If a magnet picks up stainless steel, did I buy a fake?

Not necessarily. Magnetism depends on the metallographic structure: 201, 304, 316 and 316L are austenitic and are non-magnetic in the annealed state; 430 is ferritic (no nickel) and is magnetic by nature, yet it is still real stainless steel. In addition, after cold working such as bending, cold rolling and wire drawing, part of the structure of 304 and 316 turns to martensite and may also be picked up by a magnet; the effect is clearly stronger in 304, which has a lower nickel content, than in 316. Solution annealing can remove it, but lowers strength and may cause distortion (the Australian Stainless Steel Development Association, ASSDA Technical FAQ 3). So “whether it is picked up” can tell you the structure, not whether it is genuine. If your application has a clear requirement on magnetic permeability, please say so when asking for a quotation, and take the material certificate as the reference.

› Related product: 304 Stainless Steel Window Screen Mesh (for outdoor weather resistance)

What is the difference between 304 and 316? Must I use 316?

The difference is molybdenum. 316 contains 2–3% molybdenum, and its tolerance of local pitting caused by chloride ions and of reducing acids is clearly better than 304. How to judge: if there is chlorine in the environment (seaside, chlorinated cleaning fluids, electrolytes) or acid liquids, use 316; in a dry indoor place, for general mechanism parts, 304 is enough, and changing to 316 just costs more.

When is the L (low-carbon) version necessary?

When the part is welded and still needs corrosion resistance after welding. The carbon limit is 0.07% for 304 and 0.030% for 304L. A stainless steel with higher carbon precipitates chromium carbide at the grain boundaries in the welding temperature range, which lowers corrosion resistance there (sensitization). For parts that are not welded, the ordinary version is enough.

› Related product: TIG Welding Rod (Stainless Steel / Titanium Alloy GTAW Filler)

Can 201 replace 304?

It depends on the environment. 201 replaces part of the nickel with manganese and nitrogen (Ni 3.5–5.5%, far below the 8.0–10.5% of 304), so cost is lower, but corrosion resistance is clearly weaker than 304. It can be considered for supports in indoor, dry, non-corrosive environments; whenever it will meet moisture, cleaning agents or the outdoors, using 201 in place of 304 is not recommended.

The drawing says just “stainless steel”; what should I add when asking for a quotation?

Three things are enough: the environment of use (indoor / outdoor / chlorine-containing / acid or alkali), whether it is welded, and any requirement on magnetism or surface treatment. These three decide the grade; size and tolerance are given separately. If your factory has a specified format for material certificates, please say so as well.

4. Look it up directly against your need

Your needSuggested gradeMatching item on the website
General mechanism parts, fixtures, indoor equipment304Stainless Steel Sheet, Stainless Steel Rod
Welded and still needing corrosion resistance after welding304L / 316LStainless Steel Sheet, TIG Welding Rod
Chlorine environments, chemical processing, seaside316 / 316L316L Stainless Steel Mesh, Stainless Steel Wire
Filtering, sieving, shielding mesh316LMetal Mesh Series
Outdoor insect and dust screen304304 Stainless Steel Window Screen Mesh
Indoor non-corrosive environment, cost first201Metal Rod Series

Stainless steel grade and specification check

Give the environment of use, whether it is welded, and the size and quantity together, and we can help confirm whether the grade is over-specified. Small quantities for research trials are accepted as well. Contact Jiahon for a quotation →